The nickel-metal hydride battery technical training materials provided by electronic enthusiasts for you: Nickel hydride battery principles, Nickel hydride battery technical training materials: Nickel hydride battery principles The positive active material of nickel-hydrogen batteries is nickel hydroxide (called nickel oxide electrode), and the negative active material The substance is a metal oxide, also called a hydrogen storage alloy (the electrode is called a hydrogen storage alloy)
Nickel-metal hydride battery technical training materials: Principles of nickel-metal hydride batteries
The positive active material of the nickel-hydrogen battery is nickel hydroxide (called nickel oxide electrode), the negative active material is metal oxide, also called hydrogen storage alloy (the electrode is called hydrogen storage electrode), and the electrolyte is 6N potassium hydroxide. During battery charging and discharging The battery reaction during the process is:
Among them, M represents hydrogen storage alloy material.
The open circuit voltage of the battery is: 1.2V~1.3V, which varies due to different hydrogen storage materials and preparation processes.
When overcharging, the reaction on the two poles is:
On the nickel oxide electrode: 4OH`-4e-2H2O+O2
On the hydrogen storage electrode; 2H2O+O2+4e—4OH`
Overall reaction when the battery is overcharged: O
In the design of batteries, the method of using an excessive amount of negative electrode is generally used. When the nickel oxide electrode is fully charged, oxygen is generated, which is recombined into water at the negative electrode through diffusion. In this way, the internal pressure of the battery is kept constant and the concentration of the electrolyte is kept constant. Giant changes occur.
When the battery is over-discharged, the electrode reaction is:
On nickel oxide electrode: 2H2O+2e—H2+2OH`
On the hydrogen storage electrode; H2+2OH`-2e—2H2O
Overall reaction when the battery is over-discharged: O
Although the net result of the total battery reaction is zero when over-discharged, polarity reversal will occur. Since the hydrogen produced on the positive electrode will be recombined on the negative electrode, the stability of the system is also maintained. In addition, the negative active material hydrogen can be adsorbed into the dry hydrogen storage alloy in the hydrogen atomic state at a relatively high density. On such an electrode, the hydrogen absorption and release reaction can proceed smoothly, and the discharge performance is improved compared to cadmium-nickel batteries.
Popular recommendation
801752 polymer battery.Chinese enterprises break through the core technology of high-nickel single c
2023-10-08AG4 battery.What should we pay attention to in the winding process of 18650 lithium ion battery?
2023-10-12CR2477 battery.The world's most advanced consumer-grade battery technology is here
2023-10-08AG3 battery.What is the production process of 18650 lithium battery?
2023-10-09lithuim ion battery 18650.What is the difference between 18650 lithium battery and 26650 lithium bat
2023-10-13Ni-MH battery pack.Introduction to vacuum distillation recovery technology of scrap nickel-cadmium b
2023-10-09AG1 battery!Optimistic about the performance of lithium battery materials, confirming growth and new
2023-10-08How to reduce the consumption of platinum metal in fuel power lithium battery
2022-11-04aa alkaline battery.Understand the key points of the 18650 lithium battery pack process in one artic
2023-10-093.7v 3000mah 18650 battery.Italy has developed a semi-solid lithium-oxygen battery that can be "
2023-10-0818650 battery 3500mah.Which one has better performance, polymer lithium battery or 18650 lithium bat
2023-10-133.7V Lithium Polymer Battery.[Popular Science] Research on the mechanism of 18650 battery failure ca
2023-10-09